SYSTEM

The gas-delivery system was purged for at least two minutes between subsequent welds. The welds were carried out on chemi-etched samples, with chemi-etched filler wire and using a twin-spot energy profile, based on the thus far accumulated experience. (W 354) (1)

Gas-delivery system = Sistema de saída de gás

 

This report evaluates a new high velocity flame-spray system that uses consumable in a wire form. (W 295) (2)

Flame-spray system = Sistema de pulverização de chama

 

To combat surface melting, further changes were made to the remote heating zone pattern using the deflection system. (W 225) (3)

Deflection system = Sistema de deflexão

 

(1) Achieving Low-Porosity Laser Welds in Aerospace Aluminium Alloy

G Verhaeghe and P Hilton 

TWI

S Barnes 

Warwick Manufacturing Group

Paper presented at 2003 Aerospace Manufacturing Technology Conference (AMTC), 8-12 September 2003, Montreal, Canada.

 

(2) Coatings for offshore applications by high velocity wire flame spraying

M D F Harvey, S Shrestha and A Sturgeon

Paper presented at NACE 2005 Houston, Texas, 3-7 April 2005.

 

(3) Electron beam welding of crack sensitive nickel super alloy MAR-M-002.

T. P. Mitchell, R. Sanderson, and B. G. I. Dance

TWI Ltd